UpCodes logo
Go To Full Code Chapter
Concrete (other than high early strength) shall be maintained above 50°F (10°C) and in a moist condition for at least the first seven days after placement, except when cured in accordance with Section 1905.11.3.
Upcodes Diagrams

Related Code Sections

1905.11.1 Concrete, Regular
Concrete (other than high early strength) shall be maintained above 50°F (10°C) and in a moist condition for at least the first seven days after ...
1905.11.1 Concrete, Regular
Concrete (other than high early strength) shall be maintained above 50°F (10°C) and in a moist condition for at least the first seven days after ...
1905.11.1 Concrete, Regular
Concrete (other than high early strength) shall be maintained above 50°F (10°C) and in a moist condition for at least the first seven days after ...
8.10.1.3 Two-Way Slabs,
Circular or regular polygon-shaped supports shall be treated as square supports with the same area ...